When the adjustment ring has been turned clockwise a full 2–2.5 turns and the discharge opening still cannot be held, the liners are due for replacement.
A cone crusher sets its discharge opening by screwing the adjustment ring down onto the bowl; turns multiplied by thread pitch equal the drop of the concave. The liner wears thinner a little every day, the opening grows a little every day, and recovering the gap means turning the ring further down. With a fixed thread pitch, the accumulated turns map exactly to the thickness worn off the liner — if a full 2–2.5 turns still cannot close the gap, there is no compensation margin left.
Keep daily compensation separate from the scrap criterion: turning down a little every two or three days is normal compensation; a cumulative 2–2.5 turns that still fails to hold the setting is the replacement signal. After every adjustment, measure the discharge opening once with a lead slug — do not trust the scale alone.
Shuangjin designs adjustment-ring travel and liner thickness against the same margin, so you never end up with a ring that can still turn while the liner has already reached its limit.
Applicable models: Shuangjin SK.Y, SK.D and SJ series cone crushers
Related product: SK.D multi-cylinder hydraulic cone crusher
Ask us directly. If it is a question we are asked often, it becomes the next article — and you get the answer either way.